Use some grease, they will work better and wear less. The bigger and thicker washers are a must too.
@tylererickson622
Ай бұрын
4:20 OSHA Approved
@pokegeaks2
9 ай бұрын
Using the same die for different thicknesses will have suboptimal results given the spacing for inbetween the dies is the same in design but different for each plate thickness. The material could be just fine for the application you just haven't got the right spacing for a given plate thickness.
@brianrourke3722
Жыл бұрын
The reason the finished plate is bowing, is the plastic is deforming on the final push. Hence why we use steel dimple dies. Metal to metal forms it flat.
@Kowafatcompany
3 жыл бұрын
thanks for sharing nice video
@tlntdmedia
3 жыл бұрын
Great vid
@Bravolvi
2 жыл бұрын
Did you try lubricating? It would help metal flow on PLA surface
@RJDMaskell
2 жыл бұрын
That is a great idea that I never thought of 👍 I still think 1.5 is the max thickness you would want to use it for but lubricating it will definitely help with longevity.