I can't find my purchase history but it looks like this one I randomly found from google: souq.dental/dental-clinic-supplies/burs/carbide-burs/finishing-carbide-bur-fg-016-truncated-cone-12-flutes-iso-184
@Mahmoud-cp9hu
2 жыл бұрын
At what tempreture do we heat composite ???
@protrusive
2 жыл бұрын
60 degrees is backed well in the literature
@Mahmoud-cp9hu
2 жыл бұрын
for indirect ceramic restoration do we use microhybride composite? Is that what you mentioned??
@protrusive
2 жыл бұрын
@@Mahmoud-cp9hu correct, microhybrid is what Dr Tawfik mentioned