Una roca muy bien hecha , realmente bonita gracias por enseñarla.
@mr.gardengreen7124
Жыл бұрын
I like the procedure to apply the first layer slurry, then 2nd layer is the spraying of fiber strand, rolled with rolling pin, then 3rd layer applied mix of slurry and fiber strand applied by hand laid. We used this technique to the factory I used to work . How did you avoid fast curing/drying? How do you control water temp?
@gonzalopmolina
3 жыл бұрын
Hi, this is Gonzalo from Argentina. I want to ask you two questions: 1) why when I spray vertical walls of the mould, face coat does not “stick” or is like it melt and fall down the mould on some “random” places. 2) using a smaller size of sand, results in a softer and better finish or a soft surface ir a consequence to spray technique or other factors? Thank you a lot for your help!
@TrinicLLC
3 жыл бұрын
Send your mix design to info@trinic.us and I’ll make suggestions to improve that
@gonzalopmolina
3 жыл бұрын
@@TrinicLLC hi, I just sent you an email with the required information. Thank you!
@user-ze6nu8cx8e
Жыл бұрын
Good
@saulthompson6613
2 жыл бұрын
What’s that tool you use to cut fibreglass strands?
@TrinicLLC
2 жыл бұрын
It is a concentric chopping gun. There are blades that rotate as the fiber feeds through cutting the strand.