What's the final use please? Frames, tiles ?... I like it 👏🏻💗✨
@SusanMcGarryGlass
Жыл бұрын
Jewelry
@eshrafbousabbeh1048
Жыл бұрын
Yeah 💃🏻✨
@maggiebannenberkowitz9254
Жыл бұрын
What is your firing schedules for this?? And can you fire them again once cut up??
@SusanMcGarryGlass
Жыл бұрын
I got pretty slow because it’s so many layers. About 250F to 1200F hold for 45Min. Then 9999 to 1480F hold 20 min. Then anneal. And yes, once I cut them up (on my wet saw) I will fire polish.